Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Denilub B 00U 0Mo - PBT-Z - VAMP TECH SPA

Material Data Center offers the following functions for Denilub B 00U 0Mo:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Denilub B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.019 mm/mm ASTM D 955
Mold Shrinkage, TD 0.019 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Izod impact strength, +23°C 80 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C 5 kJ/m² ISO 180/1A
ASTM Data
Tensile Modulus 2600 MPa ASTM D 638
Tensile Strength at Yield 60 MPa ASTM D 638
Elongation at Break 10 % ASTM D 638
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 264 psi 65 °C ASTM D 648
Vicat Temperature 185 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 1320 kg/m³ ASTM D 792
Characteristics
Additives
Lubricants
Special Characteristics
Flame retardant
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.